Characteristics Of Usage
1.Excellent oxidation corrosion and
abrasion resistance of the deposited weld
metal.
2. Preheat at 212-392°F and postheat
treat at 1292-1472°F due to
self-hardening.
Weld Metal Composition
Carbon 0.0 8 %
Silicon 0.70 %
Manganese 0.76 %
Chromium 12.1 %
Mechanical Properties
-S (psi) 81,221
El 24 %
PWHT 1346 °F x 1 hr S·R